How to Fix Poor Ink Adhesion and Peeling on Plastic Film Printing Machines in Nigeria

How to Fix Poor Ink Adhesion and Peeling on Plastic Film Printing Machines in Nigeria

Nothing costs a flexible packaging business in Lagos, Kano, or Aba faster than a client rejecting a whole delivery because the print scratches off. You finish a long run of pure water sachets, bread wrappers, or shopping bags, then someone rubs the film with a fingernail or takes a length of adhesive tape to it and the ink comes away. In the Nigerian packaging market, that is a direct hit: expensive polyethylene goes to scrap and the reprint burns diesel you had already budgeted elsewhere.

Why Ink Adhesion Fails on PE, PP, and BOPP Film

Ink does not bond to plastic the way it bonds to paper. PE, PP, and BOPP are smooth, non-porous, and low in surface energy, so a solvent-based ink will wet the surface poorly and sit on top of it rather than keying into it. What makes the difference is the surface energy of the film, measured in dynes per centimetre, and it has to be raised above the surface tension of the ink before printing.

That is what corona treatment does. A high-voltage discharge across the web breaks the surface molecules and leaves microscopic polar sites the ink can attach to. Without it, no ink formulation will hold on PE or BOPP for long, which is why untreated film is not worth printing at all.

Two things go wrong in local supply. Cheaper rolls are sometimes blown without adequate treatment, and treatment decays with time — faster in a hot warehouse than in a cool one. A roll that tested fine when it was made can be marginal six months later, and many shops only discover this after the ink starts flaking mid-run.

Recycled PE adds a second problem. It is widely used here to keep bag prices down, and it often carries slip agents and wax that migrate to the surface over time. Those additives sit exactly where the ink needs to bond, and they defeat treatment that would otherwise have been sufficient.

The Dyne Pen Test: Reading Surface Tension on the Roll

Test before you print, not after. A dyne pen is cheap, fast, and the closest thing to a go/no-go check on the shop floor. Draw a line across the web and read it within two seconds: if the ink holds a smooth, continuous line, the surface energy is above the pen’s rating; if it beads into droplets, it is below.

Match the pen to the substrate. For PE, a 38 dyne pen is the usual floor, and for BOPP most plants work to 38–40. If your standard pen passes but the print still peels, try one step higher rather than assuming the film is fine.

Stored rolls deserve a retest, especially in the dry season when warehouse temperatures climb. A roll that passed on arrival may not pass three months later, and the five minutes spent testing costs far less than a rejected delivery.

If a roll fails, it can often be salvaged. An inline corona treater mounted ahead of the first colour station refreshes the surface immediately before printing, and the effect holds long enough to finish the run. That is cheaper than scrapping the roll, provided the treater is working.

Verify the result properly rather than by fingernail. A tape pull or a cross-hatch tape test along the standard method (ASTM D3359) gives you a repeatable answer, and it tells you whether the failure is total or only at the edges.

Ink Chemistry, Tunnel Drying, and Corona Treater Safety

If the film tests well and the ink still flakes, look at the ink. Import costs and currency swings push local suppliers to dilute, and some mix binders that do not belong together. On top of that, operators often pour unverified thinner into the tray to make the ink flow, and that is where adhesion is lost: the resin binder is the glue, and thinning it past the manufacturer’s ratio leaves pigment with nothing to hold onto.

Drying matters just as much. Tunnels run too cold leave residual solvent trapped in the ink layer, and the print stays soft and easy to scratch even after rewinding. Run enough heat to cure the resin without melting or curling the film, and keep the exhaust pulling solvent vapour out at working capacity rather than cracking a window and hoping.

Corona performance depends on clean electrodes. Dust and oil build-up on the electrodes weaken the discharge and make treatment uneven across the web width, which shows up as adhesion that holds in the middle and fails at the edges. Cleaning is routine — but it is electrical work on a high-voltage unit.

Treat the treater as what it is. The housing should be interlocked so the discharge stops when the guard is opened, and cleaning or adjustment means isolating the supply, locking out, letting the residual charge discharge, and having a qualified electrician do the work. The unit also generates ozone, which has to be ducted outdoors rather than into the pressroom. A strong spark is not something to chase by hand on a live unit.

Test the roll, keep the treater in condition, and hold the ink to the maker’s dilution. That is what keeps a print on the film when the customer takes a nail to it.

If your plant is losing batches to flaking, or you are specifying corona treaters and press setups for Nigerian film supply, our technical team would be glad to review your setup.